Jai Enterprises is the Leading Designer of Aluminium Alloys in Coimbatore
This alloy conforms to BS:1490 1988 LM9. Castings are standardised in the as cast (M) condition, in the precipitation treated (TE) condition or in the fully heat treated (TF) condition.
% | % | % | |||
---|---|---|---|---|---|
Copper | 0.2 | Magnesium | 0.2-0.6 | Silicon | 10.0-13.0 |
Iron | 0.6 | Manganese | 0.3-0.7 | Nickel | 0.1 max |
Zinc | 0.1 | Lead | 0.1 max | Tin | 0.05 max |
Titanium | 0.2 | Aluminium | Remainder | Others each | 0.05 max |
Others total | 0.15 max |
|
M GRAVITY DIE CAST |
TF SAND CAST |
TF GRAVITY DIE CAST |
TE SAND CAST |
TEGRAVITY DIE CAST |
0.2% Proof Stress (N/mm2) |
95-120 |
220-250 |
270-280 |
110-130 |
150-170 |
Tensile Strength (N/mm2) |
190 |
240 |
295 |
170 |
230 |
Elongation (%) |
3-5 |
0-1 |
0-1 |
1.5 |
2 |
Impact Resistance Izod (Nm) |
- |
0.7 |
1.4 |
1.4 |
2 |
Brinell Hardness |
75-85 |
95 |
110 |
70 |
85 |
Modulus of Elasticity (103 N/mm2) |
- |
71 |
71 |
71 |
71 |
Shear Strength (N/mm2) |
- |
200 |
230 |
120 |
160 |
Tensile properties are unaffected by temperatures up to 150°C but prolonged heating at temperatures significantly higher reduces the strength. For example, the tensile strength of chill cast LM9-TF at 200°C (after heating for 500h) is approximately half that at room temperature, and only 25% of the original value at 250°C.
|
|
Coefficient of Thermal Expansion (per °C @ 20-100°C) |
0.000022 |
Thermal conductivity (cal/cm2/cm/°C @ 25°C) |
0.35 |
Electrical conductivity (% copper standard @ 20°C) |
38.0 |
Density (g/cm3) |
2.68 |
Freezing range (°C) approx. |
575-550 |
Very considerable tool wear occurs in machining this aluminium alloy, but there is not the same tendency to drag that occurs with high Silicon alloys containing no other alloying elements, e.g. LM6. Carbide-tipped tools with large rake angles and relatively low cutting speeds give good results. A cutting lubricant and coolant should be employed.
LM9 exhibits excellent resistance to corrosion under both ordinary atmospheric and marine conditions.
LM9 Can be anodised by any of the common processes, the resulting protective film ranging in colour from grey to dark brown, depending on the method employed.
Heat Treatment produces high strength and hardness